Gold Index: 565
POCO Magnetic Co.,Ltd [China (Mainland)]
Business Type:Manufacturer Country/Region: China (Mainland)
high current molded inductor
PIM1030R12MZ
Molded Power Inductor Operating temperature : -55℃ ~ +125℃Ambient Temperature, Maximum : 85℃Temperature Rise, Maximum: 40℃
2010-12-31
high power filtering reactor for solar inverter
PHD-R
1.iron core meterials: FeSi2.Large current3.small volume4.lower loss5.iron core reactor
magnetic block powder cores
PHD722-4-40
Magnetic Material: FeSi powderAe(cm2): 4Le(cm): 26.26Wa(cm2): 31Weight(g): 700...
magnetic powder cores
NPS-L184060
CoreLoss: LowestDCBias: BetterCurie Temp.: 450Flux Density(G): 8000Magnetic Material: FeSiAl...
magnetic iron powder cores for inductor
PPI300040
magnetic cores for AC/DC filtersDCBias: Good AL(Nh/N2): 45Perm: 40CoreLoss: Medium
magnetic power core for PFC
NPS184060
1.Magnetic Material: FeSiAl 2.Perm: 603.OD size: 1.84 inch4.Flux Density(G): 100005.DCBias: Good
2011-01-04
magnetic powder core
NPF106060
Magnetic Material: FeSiAL(nH/N2): 75Perm: 60Core OD(inch): 1.06Flux Density(G): 15000